You are welcome. I wrapped up the RH one and put photos ar the link.
These were fun, I’m glad folks got something out of the posts I made on them. I was in a downright ornery mood when I first started in on them or I probably would have posted more on how to do something with deep corrosion damage beneath blister rust. I don’t have a real junker right now but I’ll keep my eyes out for something fun that is badly corroded. There is all kinds of stuff out there on bead blasting or using coatings but that’s about it. Not that those are not perfectly acceptable methods, but draw file and block polishing can also work out in a lot of cases where people think it wouldn’t. Both of these were hit pretty hard, they came out fine.
Here are a couple photos of the RH one, the receiver got it bad. There are about 20 more at the link.